All Products
Contact Person :
amy
X2CrNiN18-10 lap joint flanges EN 10222-5 steel forged lap joint flanges 1.4311 SS Stainless Lap joint flange
Contact me for free samples and coupons.
Whatsapp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
xProduct Details
| Material | X2CrNiN18-10 | Steel Number | 1.4311 |
|---|---|---|---|
| Type | Forged Flanges | Standard | EN 1092-1, Typ 02 (04) + 32 (34) |
Product Description
| Grade : | X2CrNiN18-10 | |||||||||||||||
| Number: | 1.4311 | |||||||||||||||
| Classification: | Austenitic stainless steel | |||||||||||||||
| Density: | 7.9 g/cm ³ | |||||||||||||||
| Standard: |
|
| Particular ranges of sulphur content may provide improvement of particular properties. For machinability a controlled sulphur content of 0.015 % to 0.030% is recommended and permitted. For weldability, a controlled sulphur content of 0.008 % to 0.030 % is recommended and permitted. For polishability, a controlled sulphur content of 0.015 % max is recommended. Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. |
| C | Si | Mn | Ni | P | S | Cr | N |
| max 0.03 | max 1 | max 2 | 8.5 - 11.5 | max 0.045 | max 0.015 | 17.5 - 19.5 | 0.12 - 0.22 |
Mechanical properties of steel X2CrNiN18-10 (1.4311)
| Rm - Tensile strength (MPa) (+A) | 550-760 |
| Rm - Tensile strength (MPa) (+AT) | 550-760 |
| Rp0.2 0.2% proof strength (MPa) (+AT) | 270 |
| Rp0.2 0.2% proof strength (MPa) (+A) | 270-305 |
| KV - Impact energy (J) transverse, (+A) | +20° 60 | -196° 60 |
| KV - Impact energy (J) longitud., (+A) | +20° 100 |
| A - Min. elongation at fracture (%) (+A) | 30-40 |
| A - Min. elongation at fracture (%) longitud., (+AT) | 35-45 |
| Brinell hardness (HB): (+A) | 230 |
| Brinell hardness (HB): (+AT) | 210 |
Properties of steel X2CrNiN18-10 (1.4311)
| Resistance to intergranular corrosion: in the delivery condition - yes; in the sensitized condition - yes Steel shal not be applied at a metal temperature lower than -270 ° C |
Equivalent grades of steel X2CrNiN18-10 (1.4311)
| EU EN | USA - | Japan JIS | France AFNOR | England BS | Sweden SS | |||||