X6CrNiTiB18-10 Duplex Stainless Steel 1.4941 Welding Neck Flange Tube Sheet Flange

Product Summary
X6CrNiTiB18-10 (1.4941) duplex stainless steel flanges offer high durability, creep resistance, and excellent mechanical properties. Certified to EN standards including 10302, 10028-7, and 10216-5, these flanges ensure reliability for pressure applications and heat exchangers.

Product Details

Highlight:

X6CrNiTiB18-10 CNC machining flange

,

duplex stainless steel tube sheet flange

,

welding neck flange with heat exchanger

Material: X6CrNiTiB18-10
Steel Number: 1.4941
Type: Flanges
Stainless Flanges: Duplex Stainless Steel Flanges
Product Description
X6CrNiTiB18-10 CNC Machining Heat Exchanger Duplex Stainless Steel Hole Flange Tube Sheet Flange 1.4941 FLANGES
Material Specifications
Grade: X6CrNiTiB18-10
Number: 1.4941
Classification: Austenitic creep resisting steel
Density: 7.9 g/cm³
Standards: EN 10302:2008 Creep resisting steels, nickel and cobalt alloys
EN 10028-7:2007 Flat products made of steels for pressure purposes. Stainless steels
EN 10222-5:2000 Steel forgings for pressure purposes. Martensitic, austenitic and austenitic-ferritic stainless steels
EN 10216-5:2014 Seamless steel tubes for pressure purposes. Technical delivery conditions. Stainless steel tubes
EN 10269:1999 Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties
EN 10088-1:2005 Stainless steels. List of stainless steels
X6CrNiTiB18-10 stainless steel material composition and properties diagram
Chemical Composition (%) - EN 10302-2008
Element Content
C (Carbon) 0.04 - 0.08
Si (Silicon) max 1
Mn (Manganese) max 2
Ni (Nickel) 9 - 12
P (Phosphorus) max 0.035
S (Sulfur) max 0.015
Cr (Chromium) 17 - 19
Ti (Titanium) max 0.8 (Ti = 5 * C to 0.8)
B (Boron) 0.0015 - 0.005
Mechanical Properties
Tensile Strength (Rm) (+A):
490-710 MPa
Tensile Strength (Rm) (+AT):
490-690 MPa
0.2% Proof Strength (Rp0.2) (+A):
200-220 MPa
0.2% Proof Strength (Rp0.2) (+AT):
175-195 MPa
Impact Energy (KV) transverse (+A):
60 J at +20°C
Impact Energy (KV) longitudinal (+A):
100 J at +20°C
Min. Elongation at Fracture (A) (+A):
40%
Min. Elongation at Fracture (A) (+AT):
30-40%
Material Properties

Resistance to intergranular corrosion:

  • In the delivery condition - yes
  • In the sensitized condition - yes (EN 10028-7)
Note: Resistance to intergranular corrosion - no (EN 10216-5)
Equivalent Grades
EU EN France AFNOR
X6CrNiTiB18-10 Z6CNT18-10B
Related Products