Carbon Boiler Low Alloy Pipes P250GH 1.0460 C22.8 Durable For Pressure Equipment

Place of Origin Germany
Brand Name Globa
Certification CE, ISO , API, PED
Model Number 0.5''-48''
Minimum Order Quantity 1tons
Price 500 usd/ton
Packaging Details Standard Exported Package
Delivery Time 5 working days
Payment Terms L/C, D/A, D/P, T/T, Western Union, MoneyGram
Supply Ability 10000 tons

Contact me for free samples and coupons.

Whatsapp:0086 18588475571

Wechat: 0086 18588475571

Skype: sales10@aixton.com

If you have any concern, we provide 24-hour online help.

x
Product Details
Alloy Or Not Non-alloy Surface Treatment Customerized,Varnished,black Painted,PE Coated
Application Boiler Pipe,Fluid Pipe,Drill Pipe,Oil Pipe Technique Hot Rolled,Cold Drawn,welded Steel Pipe
Grade 20#,St37,A53(A,Q235 Surface Customers't Requirement,PE Coated,Black Painted,Paint Varnished Or Not
High Light

alloy steel seamless tubes

,

seamless alloy steel tube

Leave a Message
Product Description

What is the bolier Steel P250GH

 

 

Trade Name : p250gh , 1.0460 , cc2.8

 

 

Carbon Steel p250gh specification and Standard , Carbon Steel p250gh Chemical Composition , Carbon Steel p250ghequivalent, Carbon Steel p250gh Mechanical Properties? Carbon Steel p250gh manufacturer

 

P250GH , C22.8 , 1.0460 Bolier Steel low-alloy boiler Steel bards for operation at elevted temperatures for pressure

equipments acc to EN20173 , DIN17243

 

 

EN P250GH , Chemical Composition %

 

C: Mn: Si P S Cr Ni Mo V Nb Ti
EN P250GH , C22.8 , 1.0460
0.18-0.23

0.3

0.9

<0.4 <0.025 <0.015 <0.3 <0.3 <0.08 <0.02 <0.02 <0.03

 

DIN C22.8 , C22G2 , C22G2 Chemical Composition %

 

 

C: Mn: Si P S Cr Ni Mo V Al Cu
DIN C22.8 , C22G2 , C22G2 Chemical Composition %
0.18-0.23

0.3

0.9

<0.4 <0.025 <0.015 <0.3 <0.3 <0.08 <0.02 <0.02 <0.03

 

 

EN P265GH , 1.0425 Chemical Composition %

C: Mn: Si P S Cr Ni Mo V Al Cu
EN P265GH , 1.0425 Chemical Composition %
<0.2

0.5

1.4

<0.4 <0.030 <0.025 <0.3 <0.3 <0.08 <0.02 <0.03 >0.02
 
PN ST36K Chemical Composition %
C: Mn: Si P S Cr Ni Mo V Al Cu
PN ST36K Chemical Composition %

0.08

0.16

>0.4 0.15 - 0.35 <0.045 <0.045 <0.3 <0.3        


PN ST41 K Chemical Composition %

 

C: Mn: Si P S Cr Ni Mo V Al Cu
PN ST41 K Chemical Composition %
0.12-0.20 >0.45 0.15 - 0.35 <0.045 <0.045 <0.3 <0.3        

 

PN ST44 K Chemical Composition %

 

C: Mn: Si P S Cr Ni Mo V Al Cu
PN ST44 K Chemical Composition %
0.14 -0.22 >0.55 0.15 - 0.35 <0.045 <0.045 <0.3 <0.3      

 

P250GH , C22.8, 1.0460 +Delivery condition +N

 

Tensile Strength (Mpa) Impact Energy(J) Yield Strength(Mpa) Elongation(%)
410-540 >47 >250 >25

 

 

P250 Boiler Steel Heat Treatment : 

Normalizing at 890-950 ℃

Relief annealing at a temperature of 520--580 ℃

 

The other grades Desigantions : 

 

ST36K , ST41K , ST44K , P250GH , P235GH , P265GH , C22.8, C22G2, 1.0460, 1.0425 , P265GH , SPV355